TZM moly rod/bar molybdenum and zirconium-titanium alloy rods
TZM alloy rod, molybdenum and zirconium-titanium alloy rods, titanium zirconium molybdenum alloy bar:
TZM alloy is a molybdenum-based alloys commonly used in a high-temperature alloys containing 0.50% titanium, 0.08% zirconium, the remaining 0.02% carbon molybdenum alloy.
TZM alloy rod advantages:
1) TZM alloy has good mechanical properties, in particular its mechanical properties are better than that of pure molybdenum at high temperatures. Table 2 (Ti0.5 / Zr0.1) TZM alloy mechanical properties, Table 3 TZM (Ti0.5-Zr0.08) the tensile strength and elongation at high temperatures.
2) TZM alloy (molybdenum zirconium-titanium alloy) also has good weldability, the material can be well H11 steel welding. Meanwhile TZM alloy is resistant to liquid metals such as Zn corrosion. It is cold-worked by conventional methods. In the case of cooling lubricants available cemented carbide or high speed steel cutting tools for machining.
TZM alloy (molybdenum zirconium-titanium alloy) and physical properties of pure molybdenum compared as follows:
Material | density /g·cm-3 | Melting point /℃ | Boiling point /℃ |
TZM alloy (Ti0.5/Zr0.1) | 10.22 | 2617 | 4612 |
Mo | 10.29 | 2610 | 5560 |
Mechanical Properties of TZM alloy (molybdenum zirconium-titanium alloy) (ri0.5 / Zr0.1) as follows:
Mechanical Properties | Elongation (%) | elasticity modulus GPa | Tensile strength Mpa | yield strength Mpa | fracture toughness MP·m1/2) |
Value | <20 | 320 | 685 | 560-1150 | 5.8-29.6 |
TZM alloy (molybdenum zirconium-titanium alloy) high-temperature tensile strength and elongation:
Temperature | tensile strength(Mpa) | Elongation |
RT | 1140-1210 | 7.5-13.0 |
1000 | 700-720 | 5.2 |
1200 | 320-360 | 9.0 |
1300 | 190-210 | 11.5-13.5 |
1400 | 140-170 | 11-16 |
TZM alloy (molybdenum zirconium-titanium alloy) thermal performance and electrical properties:
Performance | coefficient of thermal expansion /K-1(20~100℃) | thermal conductivity W/m·K | Using maximum temperature in air ℃ | ResistivityΩ·m |
Value | 5.3X10-6 | 126 | 400 | (5.3~5.5)X10-8 |